title: Defects in crystals
heading: Vacancies, dislocations and traps, and what they cost a device
eyebrow: B12 · Lesson 44 · Defects in crystals
xp: 50
---

::: hook
Everything in this course assumed perfect crystals, and the real ones in a fab come remarkably close: a silicon wafer has essentially no dislocations, and its unintended impurities are below one part in 10¹². That purity is necessary because a few defects do a lot of damage. A metal atom at 10¹³ cm⁻³ can cut minority-carrier lifetime to microseconds and raise a diode's leakage a thousandfold; a lattice mismatch of under 1% between a layer and its substrate spawns dislocations every few tens of nanometers once the layer is too thick. Defect physics explains why devices leak, why LEDs grown on mismatched substrates lose light, and why fabs fight contamination so hard.
:::

::: play
- The curve is how strongly a single trap level generates and recombines carriers (Shockley–Read–Hall), relative to a trap at midgap, against its energy from the intrinsic level.
- The rate falls as $1/\cosh(\Delta E/kT)$: a trap a few tenths of an eV from midgap is thousands of times less effective. Deep, near-midgap levels (gold, iron, many dislocation states) are the killers.
- The readout gives the SRH lifetime $\tau = 1/(\sigma v_{th}N_t)$ for the trap density you set.
:::
:::

```sim plot
view: graph
x: d = -0.55..0.55 eV
y: r = 0..1.05
slider: T = 200..450 step 5 = 300 K
slider: N = 1e10..1e16 = 1e13 cm^-3 log
plot: 1/cosh(d/(0.000086173*T)) | samples: 1200 | label: rate ÷ midgap rate
readout: SRH lifetime with σ 10⁻¹⁵ cm² and v 10⁷ cm/s, µs = 1/(1e-15*1e7*N)*1e6
```

::: predict
## Silicon contains 10¹³ cm⁻³ of a midgap trap with capture cross section 10⁻¹⁵ cm². With thermal velocity 10⁷ cm/s, what's the minority-carrier lifetime?

- [ ] 1 ns
- [ ] 1 µs
- [x] 10 µs
- [ ] 1 s

::: reveal
$\tau = \frac{1}{\sigma v_{th}N_t} = \frac{1}{10^{-15} \times 10^7 \times 10^{13}}$ = 10 µs. One trap per 5 × 10⁹ silicon atoms sets it. Solar-grade silicon needs lifetimes of hundreds of microseconds, so metal contamination must be held below about 10¹¹ cm⁻³, part per trillion levels.
:::
:::

::: nameit
## Point defects

Vacancies (missing atoms), interstitials (extra atoms between sites) and substitutional impurities (dopants, or contaminants like iron and gold). Their equilibrium density follows the Boltzmann factor of their formation energy (B11.4); dopants diffuse by hopping into neighboring vacancies (B11.43).

## Deep levels and SRH recombination

An impurity with a level deep in the gap captures an electron from the conduction band and then a hole from the valence band, recombining them, or emits them in reverse, generating pairs. For a trap density $N_t$ with capture cross section σ:

$$\tau = \frac{1}{\sigma v_{th}N_t}$$

and the net rate depends on the trap energy as $\frac{1}{\cosh[(E_t - E_i)/kT]}$ in the depletion region: midgap traps dominate. Generation in a depletion region of width W gives a leakage current density

$$J_{gen} = \frac{qn_iW}{2\tau}$$

which grows with $n_i$, so it doubles about every 8 to 10 K near room temperature.

## Dislocations

Line defects, characterized by a Burgers vector b, the slip they encode. In heteroepitaxy, a layer whose lattice constant differs by a fraction f from its substrate grows strained up to a **critical thickness**, then relaxes by forming misfit dislocations spaced about b/f apart. Their cores carry dangling bonds that act as recombination centers: GaN LEDs on sapphire work despite 10⁸ to 10⁹ dislocations per cm² only because carriers in InGaAs quantum wells are localized before they find them.

## Fighting defects

Fabs use gettering (deliberately damaged or oxygen-precipitated regions that trap metals away from devices), ultra-pure chemicals, and epitaxy on matched or graded buffers. Silicon wafers are grown dislocation-free by the Czochralski method with a thin "neck" that lets dislocations grow out.
:::

::: example
## A silicon diode has a 1 µm depletion region and 10 µs lifetime. What generation current density does it leak at 300 K?

::: solution
1. **Generation current density.**
   $$\begin{aligned} J &= \frac{qn_iW}{2\tau} \\ &= \frac{1.6 \times 10^{-19} \times 10^{10} \times 10^{-4}}{2 \times 10^{-5}} \\ &= 8 \times 10^{-9}\ \text{A/cm}^2 \end{aligned}$$
2. **For a 1 mm² diode.** It leaks 80 pA, rising tenfold every 30 K or so.
3. **Where it matters.** This leakage sets the dark current of photodiodes and the hold time of DRAM cells.

**Answer:** the diode leaks $8 \times 10^{-9}$ A/cm², 80 pA for a 1 mm² diode.
:::
:::

::: example
## Si₀.₈Ge₀.₂ is grown on silicon. How far apart are misfit dislocations once it fully relaxes?

::: solution
1. **Mismatch.**
   $$\begin{aligned} f &= \frac{0.2 \times 0.0227}{0.5431} \\ &= 0.84\% \end{aligned}$$
2. **Burgers vector.** For the common 60° dislocation,
   $$\begin{aligned} b &= a/\sqrt2 \\ &= 0.384\ \text{nm} \end{aligned}$$
3. **Spacing.**
   $$\frac bf = 46\ \text{nm}$$
4. **In devices.** Strained-SiGe transistors keep the layers below the critical thickness so they never relax.

**Answer:** once the layer fully relaxes, the misfit dislocations are about 46 nm apart.
:::
:::

::: example
## Forming a vacancy in silicon costs about 3.6 eV. Ignoring the formation entropy, what's the equilibrium vacancy concentration at 1100 °C?

::: solution
1. **Thermal energy.** kT at 1373 K is 0.118 eV.
2. **Vacant fraction.**
   $$\begin{aligned} e^{-3.6/0.118} &= e^{-30.4} \\ &= 6.1 \times 10^{-14} \end{aligned}$$
3. **Concentration.** With $5 \times 10^{22}$ sites per cm³ that's $3 \times 10^9$ cm⁻³.
4. **Entropy.** The vibrational entropy of forming a vacancy raises this by a factor of 100 or more.
5. **Why it matters.** Vacancies and self-interstitials carry dopants through the crystal during annealing, which is why their concentration, and anything that disturbs it like oxidation, changes diffusion rates.

**Answer:** about $3 \times 10^9$ vacancies per cm³, a fraction $6.1 \times 10^{-14}$ of the sites.
:::
:::

::: check
given: s = 1e-16 | 1e-15 | 1e-14; v = 1.5 | 2; N = 1e11 | 1e13 | 1e15
answer: 1/(s*v*1e7*N)*1e6
unit: µs
tolerance: 0.5%

## A trap has capture cross section {s} cm², density {N} cm⁻³, and carriers move at {v} × 10⁷ cm/s. What's the SRH lifetime?

::: right
Right. $\tau = \frac{1}{\sigma v_{th}N_t}$ = {answer} µs.
:::

::: misses
- [s*v*1e7*N] That's the capture rate; the lifetime is its inverse.
- [any] Not yet. τ = 1/(σvN).
:::
:::

::: check
given: d = 0.05 | 0.15 | 0.3; T = 250 | 300 | 400
answer: 1/cosh(d/(0.000086173*T))
tolerance: 1%

## A trap sits {d} eV from the intrinsic level. How effective is it at generation, relative to a midgap trap, at {T} K?

::: right
Right. $\frac{1}{\cosh(\Delta E/kT)}$ = {answer}.
:::

::: misses
- [exp(-d/(0.000086173*T))] That's close for large ΔE, but the exact factor is $1/\cosh$, twice as large.
- [any] Not yet. SRH generation rate.
:::
:::

::: check
given: W = 0.5 | 1 | 5; t = 1 | 10 | 100; i = 1e10 | 2e6
answer: 1.602176634e-19*i*W*1e-4/(2*t*1e-6)
unit: A/cm^2
tolerance: 0.5%

## A depletion region {W} µm wide in material with $n_i$ = {i} cm⁻³ and lifetime {t} µs: what generation current density?

::: right
Right. $J = \frac{qn_iW}{2\tau}$ = {answer} A/cm².
:::

::: misses
- [1.602176634e-19*i*W*1e-4/(t*1e-6)] Include the factor 2 from the effective lifetime in depletion.
- [any] Not yet. Convert µm to cm and µs to s.
:::
:::

::: check
given: x = 0.1 | 0.2 | 0.3
answer: 0.5431/sqrt(2)/(x*0.0227/0.5431)
unit: nm
tolerance: 0.5%

## Relaxed $\text{Si}_{1-x}\text{Ge}_x$ with x = {x} on silicon: how far apart are 60° misfit dislocations (b = a/√2)?

::: right
Right. S = b/f with $f = \frac{0.0227x}{0.5431}$: {answer} nm.
:::

::: misses
- [0.5431/(x*0.0227/0.5431)] Use b = a/√2.
- [any] Not yet. Spacing = Burgers vector / mismatch.
:::
:::

::: check
given: D = 12 | 36; t = 1 | 10 | 100
answer: sqrt(D*t*1e-6)*1e4
unit: µm
tolerance: 0.5%

## Minority carriers with D = {D} cm²/s have SRH lifetime {t} µs. What's their diffusion length?

::: right
Right. $\sqrt{D\tau}$ = {answer} µm.
:::

::: misses
- [any] Not yet. Convert to cm, then µm.
:::
:::

::: check
kind: choice

## Which trap is most damaging to a silicon device's leakage current?

- [ ] A shallow donor 45 meV below the conduction band
- [x] A level near midgap, like gold's acceptor level
- [ ] A level 0.1 eV above the valence band
- [ ] None: traps don't cause leakage

::: misses
- [1] Shallow levels are ionized dopants; they don't recombine carriers effectively.
- [3] Near a band edge the trap mostly exchanges carriers with that band; generation needs both bands.
- [4] Trap-assisted generation is the main leakage source in good diodes at room temperature.
:::
:::

::: check
kind: parts
given: E = 2.5 | 3.6; T = 1000 | 1400

## Forming a vacancy in a crystal with $5 \times 10^{22}$ sites per cm³ costs {E} eV (ignore entropy).

::: part
answer: exp(-E/(0.00008617333*T))
tolerance: 1%

### What fraction of sites is vacant at {T} K?

::: misses
- [any] $e^{-E_f/kT}$.
:::
:::

::: part
answer: 5e22*exp(-E/(0.00008617333*T))
unit: cm⁻³
tolerance: 1%

### How many vacancies per cm³ is that?

::: misses
- [any] Multiply by the site density.
:::
:::
:::

::: check
kind: derivation
vars: s = 0.0000000000000001..0.000000000000001, N = 1000000000000..100000000000000, v = 1000000..20000000, D = 1..40

## Traps with cross section s (cm²) and density N (cm⁻³) capture carriers moving at v (cm/s), with diffusion constant D (cm²/s).

::: step
answer: 1/(s*N*v)

### What's the carrier lifetime?
:::

::: step
answer: sqrt(D/(s*N*v))

### What's the diffusion length, in cm?
:::

::: right
Right. Halving the trap density raises the diffusion length by √2.
:::
:::

::: explain
## Why are traps near midgap so much more effective at generating carriers than traps near a band edge?

::: model
Generating an electron–hole pair through a trap takes two steps: the trap must emit an electron to the conduction band and emit a hole to the valence band (capture an electron from it). Each emission rate falls exponentially with the energy distance to the band involved. A trap near the conduction band emits electrons easily but hole emission, across almost the whole gap, is exponentially slow, and the overall cycle is limited by its slower step. A midgap trap splits the gap into two equal steps, each about $E_g/2$, so neither is hopelessly slow, and the cycle runs fastest. That's the $1/\cosh(\Delta E/kT)$ dependence, and why deep metal impurities are watched so closely.
:::
:::

::: practice

::: check
given: s = 3e-16 | 3e-14; v = 1 | 2; N = 1e10 | 1e14
answer: 1/(s*v*1e7*N)*1e6
unit: µs
tolerance: 0.5%

## SRH lifetime: σ = {s} cm², N = {N} cm⁻³, v = {v} × 10⁷ cm/s?

::: misses
- [any] $1/\sigma vN$.
:::
:::

::: check
given: d = 0.1 | 0.4; T = 300 | 350
answer: 1/cosh(d/(0.000086173*T))
tolerance: 1%

## Relative effectiveness of a trap {d} eV from midgap at {T} K?

::: misses
- [any] $1/\cosh(\Delta E/kT)$.
:::
:::

::: check
given: W = 0.3 | 3; t = 0.5 | 50; i = 1e10 | 1e11
answer: 1.602176634e-19*i*W*1e-4/(2*t*1e-6)
unit: A/cm^2
tolerance: 0.5%

## Generation current: W = {W} µm, τ = {t} µs, $n_i$ = {i} cm⁻³?

::: misses
- [any] $qn_iW/2\tau$.
:::
:::
:::