title: Piezoelectric and ferroelectric devices
heading: Crystal resonators, actuators and sensors, and where a ferroelectric's polarization comes from
eyebrow: B12 · Lesson 43 · Piezoelectric and ferroelectric devices
xp: 50
---

::: hook
Every computer, phone and radio keeps time with a sliver of quartz that rings when a voltage squeezes it. Lesson 42 met piezoelectricity and ferroelectrics in a paragraph each; this lesson builds the circuit models engineers actually use. To an oscillator, a quartz crystal is a series RLC with an inductance of millihenries and a Q of tens of thousands, shunted by a few picofarads, and that model explains why the frequency depends on the load capacitance printed on the datasheet. The same physics stretched across a stack of ceramic layers moves a fuel injector or a disk-drive head by micrometers, and turned around it measures force. Ferroelectrics such as PZT get their huge response from a spontaneous polarization, and Landau's free-energy expansion shows where that polarization comes from and why its permittivity spikes near the Curie point.
:::

::: play
- The impedance magnitude of a 10 MHz crystal in the Butterworth–Van Dyke model: a motional branch ($R_1$ = 10 Ω, $L_1$ = 10.1 mH, $C_1$ = 25 fF) in parallel with the electrode capacitance $C_0$. The horizontal axis is the offset from the series resonance in kHz.
- At zero offset the motional branch's reactances cancel and $|Z|$ falls to $R_1$. A little higher, the motional branch looks inductive and resonates with $C_0$: the parallel (anti-)resonance, where $|Z|$ peaks.
- Raise $C_0$ and the parallel resonance moves toward the series one: the gap is about $f_s C_1/2C_0$.
:::

```sim plot
view: graph
x: d = -10..50
y: Z = 1..10M log
slider: C0 = 2..10 step 0.5 = 5
plot: 1/sqrt((10/(100 + ((1 + d*1e-4)^2 - 1)^2/(1.5707963e-6*(1 + d*1e-4))^2))^2 + (2*pi*1e7*(1 + d*1e-4)*C0*1e-12 - (((1 + d*1e-4)^2 - 1)/(1.5707963e-6*(1 + d*1e-4)))/(100 + ((1 + d*1e-4)^2 - 1)^2/(1.5707963e-6*(1 + d*1e-4))^2))^2) | label: impedance in Ω | samples: 8000
readout: parallel resonance offset (kHz) = 1e4*(sqrt(1 + 25e-15/(C0*1e-12)) - 1) | digits: 3
```

::: predict
## A 10 MHz crystal has $C_1$ = 25 fF and $C_0$ = 5 pF. It's specified for an 18 pF load capacitance, but the board's load is really 15 pF. Roughly how far off is the frequency?

- [ ] Under 1 ppm
- [x] About 80 ppm high
- [ ] About 80 ppm low
- [ ] About 0.1% high

::: reveal
In a parallel-mode oscillator, the crystal runs where its motional branch resonates with $C_0 + C_L$, which is $f_s\sqrt{1 + C_1/(C_0 + C_L)}$. The offset from $f_s$ is about $C_1/2(C_0 + C_L)$: 543 ppm at 18 pF and 625 ppm at 15 pF. The smaller load pulls the frequency up by about 80 ppm, while a typical crystal is specified to 20 or 30 ppm. That's why board designers compute the load capacitance, stray capacitance included, before choosing the two capacitors at the oscillator's pins.
:::
:::

::: nameit
## Piezoelectric constitutive equations

In a piezoelectric crystal, strain and polarization are coupled. Along one axis,

$$S = s^E T + dE, \qquad D = dT + \varepsilon^T E$$

where $S$ is strain, $T$ stress, $E$ field, $D$ displacement, $s^E$ the compliance at constant field and $d$ the piezoelectric coefficient in C/N (equivalently m/V). Read one way, a stress makes charge, $Q = dF$ for a force on a plate; read the other, a field makes strain, $\Delta t = dV$ for a voltage across a plate. The **coupling coefficient** $k$, with $k^2 = d^2/(s^E\varepsilon^T)$, is the fraction of stored energy converted between the electrical and mechanical forms. Quartz has $d_{11}$ = 2.3 pC/N and small $k$; PZT ceramics reach hundreds of pC/N and $k$ near 0.7.

Only crystals without a center of symmetry can be piezoelectric: squeezing a centrosymmetric crystal can't create a polarization that would have to point in some direction. Silicon is centrosymmetric, so silicon MEMS resonators and filters use deposited films of aluminum nitride or PZT for transduction.

## The Butterworth–Van Dyke model

Near one resonance, a piezoelectric resonator is a **motional branch** $R_1$, $L_1$, $C_1$ (the mechanical mass, compliance and loss, seen through the piezoelectric coupling) in parallel with $C_0$, the ordinary capacitance of the electrodes.

$$f_s = \frac{1}{2\pi\sqrt{L_1C_1}}, \qquad f_p = f_s\sqrt{1 + \frac{C_1}{C_0}} \approx f_s\left(1 + \frac{C_1}{2C_0}\right), \qquad Q = \frac{2\pi f_sL_1}{R_1}$$

For a thickness-mode plate at its fundamental, $C_1/C_0 = 8k^2/\pi^2$, so a weakly coupled material like quartz has its two resonances close together, and the frequency can be pulled only slightly. That's the price of its stability.

With a load capacitance $C_L$ in series, the operating frequency is

$$f_L = f_s\sqrt{1 + \frac{C_1}{C_0 + C_L}}$$

and its sensitivity, the **trim sensitivity**, is about $-\dfrac{C_1}{2(C_0 + C_L)^2}$ per farad of load.

## Ferroelectrics and Landau theory

A ferroelectric has a spontaneous polarization that an applied field can reverse. Landau expanded the free energy density in the polarization:

$$f = f_0 + \tfrac12\alpha_0(T - T_0)P^2 + \tfrac14\beta P^4 - EP$$

with $\alpha_0, \beta > 0$. Setting $\partial f/\partial P = 0$:

- Above $T_0$, the minimum at zero field is $P = 0$, and the susceptibility is $\chi = 1/(\varepsilon_0\alpha_0(T - T_0))$: the **Curie–Weiss law**, $\varepsilon_r \approx C/(T - T_0)$ with $C = 1/(\varepsilon_0\alpha_0)$.
- Below $T_0$, $P_s = \sqrt{\alpha_0(T_0 - T)/\beta}$, and the susceptibility is half what Curie–Weiss gives at the same distance from $T_0$.
- The curve $E(P) = \alpha P + \beta P^3$ with $\alpha < 0$ turns back on itself; its turning points give the intrinsic coercive field $E_c = \dfrac{2}{3\sqrt3}|\alpha|P_s$.

Measured coercive fields are far smaller than the intrinsic one, because real crystals switch by nucleating and growing domains instead of reversing everywhere at once. The permittivity peak near $T_0$ is why barium titanate capacitors (X7R and similar classes) pack so much capacitance into a small volume, and why their capacitance drifts with temperature and falls with DC bias.
:::

::: example
## A 10 MHz crystal has $R_1$ = 10 Ω, $C_1$ = 25 fF and $C_0$ = 5 pF. Find $L_1$, $Q$, the parallel resonance and the frequency offset with an 18 pF load, and its trim sensitivity there.

::: solution
1. **Motional inductance.**
   $$\begin{aligned} L_1 &= \frac{1}{(2\pi f_s)^2C_1} \\ &= \frac{1}{(6.283 \times 10^7)^2 \times 25 \times 10^{-15}} \\ &= 10.13\ \text{mH} \end{aligned}$$
2. **Quality factor.**
   $$\begin{aligned} Q &= \frac{2\pi f_sL_1}{R_1} \\ &= 63\,700 \end{aligned}$$
3. **Parallel resonance.**
   $$\begin{aligned} f_p - f_s &= f_s\left(\sqrt{1 + \frac{C_1}{C_0}} - 1\right) \\ &= 24.97\ \text{kHz} \end{aligned}$$
4. **Offset with an 18 pF load.** With $C_L$ = 18 pF, $C_0 + C_L$ = 23 pF and the crystal runs
   $$\begin{aligned} \frac{\Delta f}{f_s} &= \sqrt{1 + \frac{25 \times 10^{-15}}{23 \times 10^{-12}}} - 1 \\ &= 543\ \text{ppm} \end{aligned}$$
   above $f_s$.
5. **Trim sensitivity.**
   $$\frac{C_1}{2(C_0 + C_L)^2} = 23.6\ \text{ppm/pF}$$
6. **Why crystals win.** A millihenry-scale inductor with a Q of 60 000 is impossible to wind; the crystal gets it from mechanical motion, which is why a crystal oscillator beats any LC oscillator for stability by orders of magnitude.

**Answer:** $L_1$ = 10.13 mH and Q = 63 700, the parallel resonance is 24.97 kHz above $f_s$, and with an 18 pF load the crystal runs 543 ppm above $f_s$, with a trim sensitivity of 23.6 ppm per pF.
:::
:::

::: example
## A multilayer PZT stack actuator has 200 layers, each 100 µm thick, with $d_{33}$ = 500 pC/N. What stroke does 150 V give? And a quartz force sensor ($d_{11}$ = 2.3 pC/N) feeds a charge amplifier with a 100 pF feedback capacitor: what output does 10 N give?

::: solution
1. **Each layer.** Each layer sees the full 150 V, a field of 1.5 kV/mm, and stretches by $d_{33}V$.
2. **Stroke.**
   $$\begin{aligned} \Delta L &= n d_{33}V \\ &= 200 \times 500 \times 10^{-12} \times 150 \\ &= 15\ \mu\text{m} \end{aligned}$$
3. **Why thin layers.** The layers are electrically in parallel and mechanically in series, which is why stacks are built thin-layered: the same stroke from one 20 mm block would need 30 kV.
4. **Sensor charge.**
   $$\begin{aligned} Q &= d_{11}F \\ &= 23\ \text{pC} \end{aligned}$$
5. **Charge amplifier output.**
   $$\begin{aligned} V &= Q/C_f \\ &= 0.23\ \text{V} \end{aligned}$$
   independent of the cable's capacitance.
6. **Why charge amplifiers.** That independence is the reason piezoelectric sensors use charge amplifiers instead of voltage amplifiers, whose gain the cable capacitance would divide.

**Answer:** the stack's stroke is 15 µm at 150 V, and the sensor's charge amplifier puts out 0.23 V for 10 N.
:::
:::

::: example
## A ferroelectric follows Landau's second-order model with Curie constant $C = 1.5 \times 10^5$ K, $T_0$ = 400 K and $\beta = 10^9$ J·m⁵/C⁴. Find its permittivity 20 K above $T_0$, its spontaneous polarization at 300 K, and its intrinsic coercive field there.

::: solution
1. **Permittivity 20 K above the transition.**
   $$\begin{aligned} \varepsilon_r &\approx \frac{C}{T - T_0} \\ &= 7500 \end{aligned}$$
2. **Landau coefficient.**
   $$\begin{aligned} \alpha_0 &= \frac{1}{\varepsilon_0C} \\ &= \frac{1}{8.854 \times 10^{-12} \times 1.5 \times 10^5} \\ &= 7.53 \times 10^5\ \text{J·m/(C²·K)} \end{aligned}$$
   so at 300 K, $|\alpha| = 7.53 \times 10^7$.
3. **Spontaneous polarization.**
   $$\begin{aligned} P_s &= \sqrt{|\alpha|/\beta} \\ &= 0.274\ \text{C/m}^2 \\ &= 27.4\ \mu\text{C/cm}^2 \end{aligned}$$
4. **Coercive field.**
   $$\begin{aligned} E_c &= \frac{2}{3\sqrt3}|\alpha|P_s \\ &= 0.385 \times 7.53 \times 10^7 \times 0.274 \\ &= 7.95 \times 10^6\ \text{V/m} \\ &= 79.5\ \text{kV/cm} \end{aligned}$$
5. **Compare with real ceramics.** The polarization is close to barium titanate's, but real ceramics switch at a few kilovolts per centimeter. The intrinsic field is an upper limit that domain-wall motion undercuts.

**Answer:** the permittivity 20 K above $T_0$ is about 7500; at 300 K the spontaneous polarization is 27.4 µC/cm² and the intrinsic coercive field 79.5 kV/cm.
:::
:::

::: check
given: n = 100 | 200 | 400; d = 300 | 500 | 600; V = 60 | 100 | 150
answer: n*d*1e-12*V*1e6
unit: µm
tolerance: 0.5%

## A PZT stack has {n} layers with $d_{33}$ = {d} pC/N, each driven by {V} V. What stroke does it give, in µm?

::: right
Right. Each layer stretches by $d_{33}V$; the stack adds them: {answer}.
:::

::: misses
- [d*1e-12*V*1e6] That's one layer. All {n} layers move together.
- [n*d*1e-12*V] Convert meters to micrometers.
- [any] Not yet. $\Delta L = nd_{33}V$.
:::
:::

::: check
kind: parts
given: f = 8 | 10 | 16 | 25; C1 = 10 | 20 | 30; C0 = 3 | 5 | 7; R = 8 | 20 | 40

## A crystal has series resonance at {f} MHz, $C_1$ = {C1} fF, $C_0$ = {C0} pF and $R_1$ = {R} Ω.

::: part
answer: 1/((2*pi*f*1e6)^2*C1*1e-15)*1e3
unit: mH
tolerance: 0.5%

### What is its motional inductance, in mH?

::: misses
- [1/((f*1e6)^2*C1*1e-15)*1e3] Use $\omega = 2\pi f$.
- [any] Not yet. $L_1 = 1/(\omega_s^2C_1)$.
:::
:::

::: part
answer: 1/(2*pi*f*1e6*C1*1e-15*R)
tolerance: 0.5%

### What is its Q?

::: misses
- [2*pi*f*1e6*C1*1e-15*R] Invert it: $Q = 1/(\omega_s C_1R_1)$.
- [any] Not yet. $Q = \omega_sL_1/R_1 = 1/(\omega_sC_1R_1)$.
:::
:::

::: part
answer: f*1e3*(sqrt(1 + C1*1e-3/C0) - 1)
unit: kHz
tolerance: 0.5%

### How far above the series resonance is the parallel resonance, in kHz?

::: misses
- [f*1e3*C1*1e-3/C0] Half that: the square root gives $C_1/2C_0$.
- [any] Not yet. $f_p = f_s\sqrt{1 + C_1/C_0}$.
:::
:::

::: right
Right. Huge inductance, femtofarad capacitance and a Q in the tens of thousands, with the two resonances a fraction of a percent apart.
:::
:::

::: check
given: C1 = 10 | 20 | 30; C0 = 3 | 5 | 7; CL = 8 | 12 | 18 | 20
answer: (sqrt(1 + C1*1e-3/(C0 + CL)) - 1)*1e6
tolerance: 0.5%

## A crystal with $C_1$ = {C1} fF and $C_0$ = {C0} pF runs with a load capacitance of {CL} pF. In ppm, how far above its series resonance does it oscillate?

::: right
Right. $f_L/f_s - 1 = \sqrt{1 + C_1/(C_0 + C_L)} - 1$ = {answer} ppm.
:::

::: misses
- [(sqrt(1 + C1*1e-3/CL) - 1)*1e6] Include $C_0$: the load is in series with the motional branch, and $C_0$ sits in parallel with the load.
- [(sqrt(1 + C1*1e-3/C0) - 1)*1e6] That's the parallel resonance with no load.
- [any] Not yet. $f_L = f_s\sqrt{1 + C_1/(C_0 + C_L)}$.
:::
:::

::: check
given: F = 2 | 5 | 20; Cf = 47 | 100 | 220
answer: 2.3*F/Cf
unit: V
tolerance: 0.5%

## A quartz force sensor ($d_{11}$ = 2.3 pC/N) carries {F} N and feeds a charge amplifier with a {Cf} pF feedback capacitor. What is the output voltage's size?

::: right
Right. $Q = d_{11}F$, and the amplifier gives $Q/C_f$ = {answer}.
:::

::: misses
- [2.3*F*Cf] Divide the charge by the capacitance.
- [2.3e-12*F/Cf] Picocoulombs over picofarads is volts; the prefixes cancel.
- [any] Not yet. $V = d_{11}F/C_f$.
:::
:::

::: check
kind: parts
given: C = 1 | 1.5 | 2; dT = 50 | 100; dTa = 10 | 25

## A ferroelectric follows Landau's second-order model with Curie constant {C} × 10⁵ K and $\beta = 10^9$ J·m⁵/C⁴.

::: part
answer: C*1e5/dTa
tolerance: 0.5%

### What is its relative permittivity {dTa} K above $T_0$?

::: misses
- [C*1e5/(2*dTa)] That's the factor below $T_0$. Above, it's Curie–Weiss: $C/(T - T_0)$.
- [any] Not yet. $\varepsilon_r \approx C/(T - T_0)$.
:::
:::

::: part
answer: sqrt(dT/(8.854e-12*C*1e5)/1e9)*100
unit: µC/cm²
tolerance: 0.5%

### What is its spontaneous polarization {dT} K below $T_0$, in µC/cm²?

::: misses
- [sqrt(dT/(8.854e-12*C*1e5)/1e9)] 1 C/m² is 100 µC/cm².
- [dT/(8.854e-12*C*1e5)/1e9*100] Take the square root: $P_s = \sqrt{|\alpha|/\beta}$.
- [any] Not yet. $|\alpha| = (T_0 - T)/(\varepsilon_0C)$ and $P_s = \sqrt{|\alpha|/\beta}$.
:::
:::

::: right
Right. The permittivity diverges as $1/(T - T_0)$ above the transition, and the polarization grows as $\sqrt{T_0 - T}$ below it.
:::
:::

::: check
kind: choice

## A designer wants a piezoelectric resonator on a silicon MEMS chip. Why can't the silicon itself be the piezoelectric?

- [x] Silicon's crystal has a center of symmetry, so stress can't polarize it
- [ ] Silicon conducts too well to hold a field
- [ ] Silicon is too stiff to strain measurably
- [ ] Silicon's piezoelectric coefficient is positive but too small to use

::: right
Right. Diamond-structure silicon is centrosymmetric, so every piezoelectric coefficient is exactly zero. Films of AlN or PZT on top do the transduction, while the silicon provides the mechanics.
:::

::: misses
- [2] Intrinsic or lightly doped silicon can hold a field. The issue is symmetry.
- [3] Silicon strains like any solid; it just doesn't polarize when it does.
- [4] It's exactly zero, by symmetry, not merely small.
:::
:::

::: check
kind: derivation
vars: a = 1e5..1e6, b = 5e8..5e9, t = 10..200

## Landau's free energy is $f = \tfrac12\alpha P^2 + \tfrac14\beta P^4 - EP$ with $\alpha = -a t$ below the transition ($a$ = $\alpha_0$, $t = T_0 - T$).

::: step
answer: sqrt(a*t/b)

### Set $E = 0$ and minimize. What is $P_s$?
:::

::: step
answer: sqrt(a*t/(3*b))

### The field $E = \alpha P + \beta P^3$ has turning points where $dE/dP = 0$. At what $P$?
:::

::: step
answer: 2/3*a*t*sqrt(a*t/(3*b))

### What is the size of $E$ there, the intrinsic coercive field?
:::

::: right
Right. $E_c = \frac{2}{3\sqrt3}|\alpha|P_s$: beyond it, the polarization has nowhere to go but to flip.
:::
:::

::: check
kind: python
given: f0 = 10 | 20; C1 = 15 | 25; C0 = 4 | 6

## Model a crystal in Python. `f0` = {f0} MHz is the series resonance, `C1` = {C1} fF and `C0` = {C0} pF, with $R_1$ = 10 Ω. Write `bvd(f)` returning the complex impedance at frequency `f` in Hz; set `L1` in henries, `fp` (the exact lossless parallel resonance, Hz), and write `pull_ppm(CL)` giving the exact offset above `f0` in ppm for a load capacitance `CL` in pF.

```python starter
import math
L1 = 1 / ((2 * math.pi * f0 * 1e6) ** 2 * C1 * 1e-15)
fp = f0 * 1e6 * (1 + C1 * 1e-3 / (2 * C0))
def bvd(f):
    return 10.0
def pull_ppm(CL):
    return C1 * 1e-3 / (2 * (C0 + CL)) * 1e6
print(L1, fp)
```

```python solution
import math
fs = f0 * 1e6
c1, c0 = C1 * 1e-15, C0 * 1e-12
L1 = 1 / ((2 * math.pi * fs) ** 2 * c1)
fp = fs * math.sqrt(1 + c1 / c0)
def bvd(f):
    w = 2 * math.pi * f
    zm = 10 + 1j * (w * L1 - 1 / (w * c1))
    z0 = 1 / (1j * w * c0)
    return zm * z0 / (zm + z0)
def pull_ppm(CL):
    return (math.sqrt(1 + c1 / (c0 + CL * 1e-12)) - 1) * 1e6
print(L1, fp, abs(bvd(fs)), abs(bvd(fp)))
```

```python tests
import math
fs, c1, c0 = f0 * 1e6, C1 * 1e-15, C0 * 1e-12
assert abs(L1 * (2 * math.pi * fs) ** 2 * c1 - 1) < 1e-9, "L1 should resonate with C1 at f0."
assert abs(fp / (fs * math.sqrt(1 + c1 / c0)) - 1) < 1e-12, "fp should be the exact f0·sqrt(1 + C1/C0), not the first-order approximation."
for f in (0.9 * fs, fs, 1.001 * fs, 1.1 * fs):
    w = 2 * math.pi * f
    zm = 10 + 1j * (w * L1 - 1 / (w * c1))
    ref = 1 / (1 / zm + 1j * w * c0)
    assert abs(bvd(f) - ref) < 1e-9 * abs(ref), f"bvd({f:.6g}) should be the motional branch in parallel with C0."
for CL in (8, 18, 30):
    ref = (math.sqrt(1 + c1 / (c0 + CL * 1e-12)) - 1) * 1e6
    assert abs(pull_ppm(CL) - ref) < 1e-9 * ref, f"pull_ppm({CL}) should be {ref:.6f}, the exact value."
assert abs(bvd(fp)) > 1000 * abs(bvd(fs)), "The impedance should peak near fp and dip near f0."
```

::: right
Right. The first-order formulas are good to a few parts per million here, which is the same order as the tolerances crystals are sold to, so frequency-planning tools use the exact ones.
:::
:::

::: explain
## Why does a crystal oscillator's frequency depend on the load capacitance, and why does a quartz crystal let the designer pull it only a little, compared with a ceramic resonator?

::: model
In a parallel-mode oscillator, the crystal's motional branch $L_1C_1$ resonates in series with $C_0 + C_L$, the electrode capacitance plus the circuit's load. That combination is smaller than $C_1$ alone would be in series with nothing, so the frequency rises above the series resonance by about $C_1/2(C_0 + C_L)$, and changing $C_L$ changes it. How large that offset can be depends on $C_1/C_0$, which for a thickness-mode resonator is $8k^2/\pi^2$, with $k$ the coupling coefficient. Quartz couples weakly, so $C_1$ is a tiny fraction of $C_0$, the frequency moves only hundreds of ppm across the whole range of loads, and stray capacitance barely disturbs it. A PZT-type ceramic resonator couples strongly, so its $C_1/C_0$ is much larger: it can be pulled much further, but for the same reason its frequency is far less stable.
:::
:::

::: practice

::: check
given: d = 100 | 300 | 600; V = 10 | 50
answer: d*V*1e-3
unit: nm
tolerance: 0.5%

## A piezoelectric plate with $d_{33}$ = {d} pC/N has {V} V across it. How much does its thickness change, in nm?

::: misses
- [d*V] pC/N is pm/V; convert picometers to nanometers.
- [any] $\Delta t = d_{33}V$.
:::
:::

::: check
given: f = 4 | 12 | 32; C1 = 5 | 15; C0 = 2 | 4
answer: f*1e3*(sqrt(1 + C1*1e-3/C0) - 1)
tolerance: 0.5%

## A crystal at {f} MHz has $C_1$ = {C1} fF and $C_0$ = {C0} pF. How many kHz separate its series and parallel resonances?

::: misses
- [f*1e3*C1*1e-3/C0] That's twice the gap; take the square root.
- [any] $f_p - f_s = f_s(\sqrt{1 + C_1/C_0} - 1)$.
:::
:::
:::