D6 · Lesson 1 · Crystals and purity
Silicon's diamond-cubic crystal and its atom density, why doping at a few parts per million controls conductivity, resistivity against doping, how purity is measured in nines, growing single-crystal ingots and how dopants spread along them, and how many chips fit on a wafer
The silicon in a chip is among the purest materials humans make: electronic-grade polysilicon has about one stray atom in a hundred billion. Then, having purified it so carefully, engineers deliberately add impurities, a few atoms of boron or phosphorus per million silicon atoms, and those few atoms change the conductivity by a factor of a hundred thousand or more. Semiconductor technology rests on both feats: making a perfect crystal, and then controlling its imperfections exactly.
- The resistivity of n-type silicon against its donor concentration, , with the electron mobility falling at high doping as impurities scatter the electrons (the fit from B9: cm²/V·s).
- Pure silicon, with only cm⁻³ intrinsic carriers, has a resistivity of about 340 kΩ·cm; doping spans ten orders of magnitude below that.
- The readouts give the resistivity and how many silicon atoms there are per dopant atom.
Predict
A wafer is doped with phosphorus atoms per cm³. Silicon has atoms per cm³. What fraction of the atoms are phosphorus?
: one atom in five million, 0.2 parts per million. That tiny fraction gives an electron density a million times the intrinsic cm⁻³ and a resistivity of about 0.5 Ω·cm, nearly a million times lower than pure silicon's.
Name it
The crystal
Silicon crystallizes in the diamond-cubic lattice: each atom bonds covalently to four neighbors at the corners of a tetrahedron, with 8 atoms per cubic cell of side 5.431 Å, so
Doping and resistivity
Each phosphorus (group V) donor contributes an electron; each boron (group III) acceptor a hole. With donors fully ionized,
where the mobility falls at high doping. Doping is quoted in atoms per cm³ from about (lightly doped substrates) to (contacts and source/drain regions).
Purity
Electronic-grade polysilicon is about 99.999999999% pure, "eleven nines". Metal impurities such as iron and gold are especially harmful, since they create states in the middle of the band gap that speed up recombination (B9).
Growing the crystal
The Czochralski method dips a seed crystal into molten silicon and slowly pulls and rotates it, growing an ingot up to 300 mm across. Dopants prefer the melt to the solid by a segregation coefficient (0.8 for boron, 0.35 for phosphorus), so the melt gets richer as it's used up and the dopant concentration rises along the ingot:
where is the starting melt concentration and f the fraction already solidified.
Wafers and dies
A wafer of diameter d holds about
square dies of area A, the second term counting the partial dies lost at the edge.
Worked example
What's the resistivity of silicon with and with donors per cm³?
Show the solution
- At cm⁻³. The mobility is = 1248 cm²/V·s:
- At cm⁻³. The mobility falls to 263 cm²/V·s:
- Compare. A hundred times the doping lowers the resistivity only 21 times.
Answer 0.50 Ω·cm with donors per cm³ and 0.0237 Ω·cm with .
Worked example
How many 100 mm² dies fit on a 300 mm wafer? How does phosphorus concentration change halfway along an ingot?
Show the solution
- Dies on the wafer. The wafer's area over the die area, less the partial dies lost at the edge:
- Phosphorus halfway along. At f = 0.5:
- Compare with the start. Against 0.35 at the start, that's 57% more.
Answer 640 dies fit, and halfway along the ingot the phosphorus concentration is 0.549 , 57% more than at the start.
Worked example
Electronic-grade silicon is "nine nines" pure: one foreign atom in . Silicon has atoms per cm³. How many impurity atoms is that per cm³, and why does it matter?
Show the solution
- Impurity atoms.
- Compare with doping. That's comparable to the lightest deliberate doping, about to cm⁻³, so impurities that act as donors or acceptors would compete with the doping.
- Solar grade. Solar-grade silicon tolerates more; chips need the nine nines.
Answer impurity atoms per cm³, enough to compete with the lightest doping.
Check
Silicon is doped with atoms per cm³. How many silicon atoms are there per dopant atom?
Check
n-type silicon has donors per cm³ and an electron mobility of 1300 cm²/V·s. What's its resistivity?
Write units the way you normally would: 1.5 Ω·cm, 1500 mΩ·cm and 0.0015 kΩ·cm are the same answer.
Check
A dopant with segregation coefficient 0.35 is grown into an ingot. Once a fraction 0.25 has solidified, what's the concentration in the crystal, as a multiple of the starting melt's?
Check
About how many 25 mm² dies fit on a 200 mm wafer?
Check
Silicon has cm⁻³ donors with N = 5, and its electron mobility there is 1248 cm²/V·s.
(a)
What is its resistivity?
Write units the way you normally would: 1.5 Ω·cm, 1500 mΩ·cm and 0.0015 kΩ·cm are the same answer.
(b)
What is the sheet resistance of a 500 µm thick wafer of it?
Check
A 200 mm wafer is cut into dies of 50 mm².
(a)
About how many whole dies fit (area ÷ die, less the edge loss )?
(b)
What share of the wafer's area do they use?
Explain why
Why do a few parts per million of dopant change silicon's conductivity so dramatically?
Pure silicon at room temperature has very few free carriers, about ten billion electrons per cubic centimeter, because almost every electron is locked into the covalent bonds and few have enough thermal energy to break free across the band gap. A phosphorus atom in the lattice uses four of its five valence electrons for bonds, and the fifth is so weakly held that at room temperature it's almost always free to conduct. Adding just one phosphorus atom per five million silicon atoms therefore supplies ten quadrillion free electrons per cubic centimeter, a million times more than the intrinsic carriers, and the conductivity rises in proportion.
Practice
Keep practicing
8 kinds of problem on this topic, dealt one at a time with new numbers every time, for as long as you like.