title: Crystals and purity
heading: Silicon's diamond-cubic crystal and its atom density, why doping at a few parts per million controls conductivity, resistivity against doping, how purity is measured in nines, growing single-crystal ingots and how dopants spread along them, and how many chips fit on a wafer
eyebrow: D6 · Lesson 1 · Crystals and purity
xp: 40
---

::: hook
The silicon in a chip is among the purest materials humans make: electronic-grade polysilicon has about one stray atom in a hundred billion. Then, having purified it so carefully, engineers deliberately add impurities, a few atoms of boron or phosphorus per million silicon atoms, and those few atoms change the conductivity by a factor of a hundred thousand or more. Semiconductor technology rests on both feats: making a perfect crystal, and then controlling its imperfections exactly.
:::

::: play
- The resistivity of n-type silicon against its donor concentration, $\rho = 1/(qN_D\mu_n)$, with the electron mobility falling at high doping as impurities scatter the electrons (the fit from B9: $\mu_n = 92 + 1268/(1 + (N/1.3 \times 10^{17})^{0.91})$ cm²/V·s).
- Pure silicon, with only $10^{10}$ cm⁻³ intrinsic carriers, has a resistivity of about 340 kΩ·cm; doping spans ten orders of magnitude below that.
- The readouts give the resistivity and how many silicon atoms there are per dopant atom.
:::

```sim plot
view: graph
x: N = 1e13..1e20 log
y: r = 0.0001..10000 log
slider: D = 13..20 step 0.1 = 16
plot: 1/(1.602e-19*N*(92 + 1268/(1 + (N/1.3e17)^0.91))) | samples: 300 | label: resistivity, Ω·cm (N in cm⁻³)
marker: x = 10^D | label: your doping
readout: resistivity, Ω·cm = 1/(1.602e-19*10^D*(92 + 1268/(1 + (10^D/1.3e17)^0.91))) | digits: 3
readout: silicon atoms per donor = 5e22/10^D | digits: 3
```

::: predict
## A wafer is doped with $10^{16}$ phosphorus atoms per cm³. Silicon has $5 \times 10^{22}$ atoms per cm³. What fraction of the atoms are phosphorus?

- [ ] 1 in 1000
- [ ] 1 in 50,000
- [x] 1 in 5 million
- [ ] 1 in 5 billion

::: reveal
$5 \times 10^{22}/10^{16} = 5 \times 10^6$: one atom in five million, 0.2 parts per million. That tiny fraction gives an electron density a million times the intrinsic $10^{10}$ cm⁻³ and a resistivity of about 0.5 Ω·cm, nearly a million times lower than pure silicon's.
:::
:::

::: nameit
## The crystal

Silicon crystallizes in the **diamond-cubic** lattice: each atom bonds covalently to four neighbors at the corners of a tetrahedron, with 8 atoms per cubic cell of side 5.431 Å, so

$$n_\text{Si} = \frac{8}{(5.431 \times 10^{-8}\text{ cm})^3} = 5.0 \times 10^{22}\text{ cm}^{-3}$$

## Doping and resistivity

Each phosphorus (group V) donor contributes an electron; each boron (group III) acceptor a hole. With $N_D$ donors fully ionized,

$$\rho = \frac{1}{qN_D\mu_n}$$

where the mobility falls at high doping. Doping is quoted in atoms per cm³ from about $10^{14}$ (lightly doped substrates) to $10^{20}$ (contacts and source/drain regions).

## Purity

Electronic-grade polysilicon is about 99.999999999% pure, "eleven nines". Metal impurities such as iron and gold are especially harmful, since they create states in the middle of the band gap that speed up recombination (B9).

## Growing the crystal

The **Czochralski** method dips a seed crystal into molten silicon and slowly pulls and rotates it, growing an ingot up to 300 mm across. Dopants prefer the melt to the solid by a **segregation coefficient** $k_0$ (0.8 for boron, 0.35 for phosphorus), so the melt gets richer as it's used up and the dopant concentration rises along the ingot:

$$C_s = k_0C_0(1 - f)^{k_0 - 1}$$

where $C_0$ is the starting melt concentration and f the fraction already solidified.

## Wafers and dies

A wafer of diameter d holds about

$$\frac{\pi(d/2)^2}{A} - \frac{\pi d}{\sqrt{2A}}$$

square dies of area A, the second term counting the partial dies lost at the edge.
:::

::: example
## What's the resistivity of silicon with $10^{16}$ and with $10^{18}$ donors per cm³?

::: solution
1. **At $10^{16}$ cm⁻³.** The mobility is $\mu_n$ = 1248 cm²/V·s:
   $$\begin{aligned} \rho &= \frac{1}{qN_D\mu_n} \\ &= \frac{1}{(1.602 \times 10^{-19})(10^{16})(1248)} \\ &= 0.50\ \Omega\cdot\text{cm} \end{aligned}$$
2. **At $10^{18}$ cm⁻³.** The mobility falls to 263 cm²/V·s:
   $$\rho = 0.0237\ \Omega\cdot\text{cm}$$
3. **Compare.** A hundred times the doping lowers the resistivity only 21 times.

**Answer:** 0.50 Ω·cm with $10^{16}$ donors per cm³ and 0.0237 Ω·cm with $10^{18}$.
:::
:::

::: example
## How many 100 mm² dies fit on a 300 mm wafer? How does phosphorus concentration change halfway along an ingot?

::: solution
1. **Dies on the wafer.** The wafer's area over the die area, less the partial dies lost at the edge:
   $$\begin{aligned} N &= \frac{\pi \times 150^2}{100} - \frac{\pi \times 300}{\sqrt{200}} \\ &= 706.9 - 66.6 \\ &= 640\ \text{dies} \end{aligned}$$
2. **Phosphorus halfway along.** At f = 0.5:
   $$\begin{aligned} C_s &= 0.35C_0 \times 0.5^{-0.65} \\ &= 0.549\,C_0 \end{aligned}$$
3. **Compare with the start.** Against 0.35 $C_0$ at the start, that's 57% more.

**Answer:** 640 dies fit, and halfway along the ingot the phosphorus concentration is 0.549 $C_0$, 57% more than at the start.
:::
:::

::: example
## Electronic-grade silicon is "nine nines" pure: one foreign atom in $10^9$. Silicon has $5 \times 10^{22}$ atoms per cm³. How many impurity atoms is that per cm³, and why does it matter?

::: solution
1. **Impurity atoms.**
   $$\begin{aligned} &5 \times 10^{22} \times 10^{-9} \\ &= 5 \times 10^{13}\ \text{cm}^{-3} \end{aligned}$$
2. **Compare with doping.** That's comparable to the lightest deliberate doping, about $10^{14}$ to $10^{15}$ cm⁻³, so impurities that act as donors or acceptors would compete with the doping.
3. **Solar grade.** Solar-grade silicon tolerates more; chips need the nine nines.

**Answer:** $5 \times 10^{13}$ impurity atoms per cm³, enough to compete with the lightest doping.
:::
:::

::: check
given: e = 14 | 15 | 17 | 19
answer: 5e22/10^e
tolerance: 0.5%

## Silicon is doped with $10^{\given{e}}$ atoms per cm³. How many silicon atoms are there per dopant atom?

::: right
Right. $5 \times 10^{22}/N$ = {answer}.
:::

::: misses
- [any] Not yet. Silicon's atom density over the doping.
:::
:::

::: check
given: e = 15 | 16 | 17; m = 1300 | 1250 | 800
answer: 1/(1.602e-19*10^e*m)
unit: Ω·cm
tolerance: 0.5%

## n-type silicon has $10^{\given{e}}$ donors per cm³ and an electron mobility of {m} cm²/V·s. What's its resistivity?

::: right
Right. $1/(qN_D\mu_n)$ = {answer} Ω·cm.
:::

::: misses
- [1.602e-19*10^e*m] That's the conductivity; resistivity is its reciprocal.
- [any] Not yet. $\rho = 1/(qn\mu)$.
:::
:::

::: check
given: k = 0.35 | 0.8; f = 0.25 | 0.5 | 0.8
answer: k*(1 - f)^(k - 1)
tolerance: 0.5%

## A dopant with segregation coefficient {k} is grown into an ingot. Once a fraction {f} has solidified, what's the concentration in the crystal, as a multiple of the starting melt's?

::: right
Right. $k_0(1 - f)^{k_0 - 1}$ = {answer} times $C_0$.
:::

::: misses
- [k] That's the very first crystal; the melt has since grown richer.
- [any] Not yet. The Scheil equation.
:::
:::

::: check
given: d = 200 | 300; A = 25 | 100 | 400
answer: pi*(d/2)^2/A - pi*d/sqrt(2*A)
tolerance: 0.5%

## About how many {A} mm² dies fit on a {d} mm wafer?

::: right
Right. $\pi(d/2)^2/A - \pi d/\sqrt{2A}$ = {answer}.
:::

::: misses
- [pi*(d/2)^2/A] Subtract the partial dies around the edge.
- [any] Not yet. Wafer area over die area, less the edge.
:::
:::

::: check
kind: parts
given: N = 1 | 5 | 20; u = 1248 | 1000 | 600

## Silicon has $N \times 10^{15}$ cm⁻³ donors with N = {N}, and its electron mobility there is {u} cm²/V·s.

::: part
answer: 1/(1.602e-19*N*1e15*u)
unit: Ω·cm
tolerance: 0.5%

### What is its resistivity?

::: misses
- [any] $1/(qN\mu)$.
:::
:::

::: part
answer: 1/(1.602e-19*N*1e15*u)/(500e-4)
unit: Ω
tolerance: 0.5%

### What is the sheet resistance of a 500 µm thick wafer of it?

::: misses
- [any] ρ ÷ thickness.
:::
:::
:::

::: check
kind: parts
given: D = 200 | 300; A = 50 | 100 | 400

## A {D} mm wafer is cut into dies of {A} mm².

::: part
answer: floor(pi*(D/2)^2/A - pi*D/sqrt(2*A))
tolerance: 0

### About how many whole dies fit (area ÷ die, less the edge loss $\pi d/\sqrt{2A}$)?

::: misses
- [floor(pi*(D/2)^2/A)] Dies at the edge are lost.
- [any] $\pi r^2/A - \pi d/\sqrt{2A}$, rounded down.
:::
:::

::: part
answer: floor(pi*(D/2)^2/A - pi*D/sqrt(2*A))*A/(pi*(D/2)^2)*100
unit: %
tolerance: 0.5%

### What share of the wafer's area do they use?

::: misses
- [any] Dies × area ÷ wafer area.
:::
:::
:::

::: explain
## Why do a few parts per million of dopant change silicon's conductivity so dramatically?

::: model
Pure silicon at room temperature has very few free carriers, about ten billion electrons per cubic centimeter, because almost every electron is locked into the covalent bonds and few have enough thermal energy to break free across the band gap. A phosphorus atom in the lattice uses four of its five valence electrons for bonds, and the fifth is so weakly held that at room temperature it's almost always free to conduct. Adding just one phosphorus atom per five million silicon atoms therefore supplies ten quadrillion free electrons per cubic centimeter, a million times more than the intrinsic carriers, and the conductivity rises in proportion.
:::
:::

::: practice

::: check
given: e = 14 | 15 | 16 | 17 | 18 | 19 | 20; m = 100 | 1400
answer: 1/(1.602e-19*10^e*m)
unit: Ω·cm
tolerance: 0.5%

## Resistivity: $10^{\given{e}}$ cm⁻³, μ = {m}?

::: misses
- [any] $1/(qN\mu)$.
:::
:::

::: check
given: d = 100 | 150 | 200 | 300 | 450; A = 1 | 800
answer: pi*(d/2)^2/A - pi*d/sqrt(2*A)
tolerance: 0.5%

## Dies of {A} mm² on a {d} mm wafer?

::: misses
- [any] $\pi(d/2)^2/A - \pi d/\sqrt{2A}$.
:::
:::
:::