title: FinFET, GAA and the limits of scaling
heading: Why shrinking a planar transistor stopped working, subthreshold swing and the 60 mV per decade floor, leakage against threshold voltage, gates that wrap the channel (FinFETs and gate-all-around nanosheets), high-κ dielectrics and equivalent oxide thickness, and what limits scaling now
eyebrow: D6 · Lesson 7 · FinFET, GAA and the limits of scaling
xp: 40
---

::: hook
By the mid-2000s, transistors had a problem: they wouldn't turn off. As channels shrank below about 30 nm, the drain's field reached under the gate and held the channel partly open, and lowering the supply voltage meant lowering the threshold, which let still more current leak. A chip with a billion transistors each leaking a few nanoamperes burns watts doing nothing. The industry's answer was to change the transistor's shape: stand the channel up as a thin fin and wrap the gate around it, so the gate controls the channel from three sides, and now from all four.
:::

::: play
- Drain current against gate voltage on a log scale for a transistor with threshold $V_T$ and subthreshold swing SS (millivolts per decade of current), with 1 µA per µm of width defined as the threshold current.
- Below threshold the current falls by ten for every SS millivolts. A steeper slope (smaller SS) gives a much lower off current at the same threshold.
- No transistor that works by thermal emission over a barrier can beat 60 mV per decade at room temperature.
:::

```sim plot
view: graph
x: v = 0..0.8
y: I = 1e-13..1e-2 log
slider: T = 0.15..0.5 step 0.01 = 0.3
slider: S = 60..120 step 1 = 65
plot: 1e-6*10^((v - T)/(S/1000))/(1 + 1e-6*10^((v - T)/(S/1000))/1e-3) | samples: 400 | label: drain current, A/µm (v = gate voltage)
marker: x = T | label: threshold
readout: off current at 0 V, A/µm = 1e-6*10^(-T/(S/1000)) | digits: 3
readout: on/off ratio at 0.7 V = 1e-6*10^((0.7 - T)/(S/1000))/(1 + 1e-6*10^((0.7 - T)/(S/1000))/1e-3)/(1e-6*10^(-T/(S/1000))) | digits: 3
```

::: predict
## A transistor has a threshold of 0.3 V (defined at 1 µA/µm) and a subthreshold swing of 65 mV/decade. What does it leak with the gate at 0 V?

- [ ] About 1 µA/µm
- [ ] About 1 nA/µm
- [x] About 24 pA/µm
- [ ] Nothing

::: reveal
From the threshold down to 0 V is 300 mV, which is 300/65 = 4.6 decades: $10^{-6} \times 10^{-4.6}$ = 2.4 × 10⁻¹¹ A/µm, or 24 pA/µm. With a sloppy 90 mV/decade the same threshold leaks 460 pA/µm, about nineteen times more. A billion transistors of 0.1 µm width each at 24 pA/µm and 0.7 V waste 1.7 mW; at 460 pA/µm, 32 mW.
:::
:::

::: nameit
## Subthreshold swing

Below threshold, current flows by electrons diffusing over a barrier that the gate lowers, so it grows exponentially with gate voltage. The **subthreshold swing** is the gate voltage needed for a tenfold change:

$$SS = \frac{kT}{q}\ln 10\left(1 + \frac{C_d}{C_\text{ox}}\right) \ge 59.5 \text{ mV/decade at 300 K}$$

where $C_d$ is the depletion capacitance that steals some of the gate's control. The off current is $I_\text{off} = I_T \times 10^{-V_T/SS}$, so every SS millivolts of threshold reduction costs ten times more leakage. That's why supply voltages stalled near 0.7 V.

## Short-channel effects

In a short channel the drain's field lowers the source barrier (**drain-induced barrier lowering**), and the threshold falls as the gate length shrinks. The gate keeps control only if the channel is much thinner than it is long. For a channel of thickness $t_\text{Si}$ gated from both sides, the **natural length** $\lambda = \sqrt{\varepsilon_\text{Si}t_\text{Si}t_\text{ox}/(2\varepsilon_\text{ox})}$ should be at most about a fifth of the gate length.

## FinFETs and nanosheets

- A **FinFET** (from 2011) stands the channel up as a fin a few nanometers thick with the gate on three sides. Its effective width is $2H_\text{fin} + W_\text{fin}$ per fin, so drive current is set by fin height and count.
- **Gate-all-around** nanosheets (from about 2022) stack horizontal sheets with the gate surrounding each, adding $2(W + T)$ of width per sheet.

## High-κ gates

Below about 1.2 nm, SiO₂ leaks badly by tunneling. Hafnium oxide (κ ≈ 22) gives the same capacitance in a physically thicker film; its **equivalent oxide thickness** is $t_\text{EOT} = t_\text{high-κ} \times 3.9/\kappa$.

## The limits now

Atoms (silicon's lattice spacing is 0.54 nm), the cost of lithography, the resistance of ever-thinner wires, heat, and the 60 mV/decade floor. Designers now gain more from stacking, packaging and specialized circuits than from shrinking.
:::

::: example
## Find the natural length of a fin 7 nm thick with 1 nm of oxide, and the effective widths of a 50 nm tall fin and of three 30 × 5 nm nanosheets.

::: solution
1. **Natural length.**
   $$\begin{aligned} \lambda &= \sqrt{\frac{11.7 \times 7 \times 1}{2 \times 3.9}}\ \text{nm} \\ &= 3.24\ \text{nm} \end{aligned}$$
   so gate lengths down to about 16 nm stay well controlled.
2. **Fin width.** Both sides and the top:
   $$2 \times 50 + 7 = 107\ \text{nm}$$
3. **Nanosheet width.** Around each of the three sheets:
   $$3 \times 2 \times (30 + 5) = 210\ \text{nm}$$
   in about the same footprint.

**Answer:** λ = 3.24 nm; the fin gives 107 nm of effective width and the three nanosheets 210 nm.
:::
:::

::: example
## What's the swing limit at 77 K and at 100 °C? What EOT does 2 nm of HfO₂ give?

::: solution
1. **Swing at 77 K.**
   $$\frac{kT}{q}\ln 10 = 15.3\ \text{mV/decade}$$
2. **Swing at 100 °C.** At 373 K it's 74.0 mV/decade.
3. **What that means.** Cold transistors switch far more sharply, hot ones leak more.
4. **EOT of 2 nm of HfO₂.**
   $$2\ \text{nm} \times \frac{3.9}{22} = 0.35\ \text{nm}$$

**Answer:** the limit is 15.3 mV/decade at 77 K and 74.0 mV/decade at 100 °C, and 2 nm of HfO₂ has an EOT of 0.35 nm.
:::
:::

::: example
## A designer lowers a transistor's threshold by 100 mV to make it faster. With an 80 mV/decade subthreshold swing, how much more does it leak?

::: solution
1. **Extra leakage.**
   $$10^{100/80} = 17.8$$
2. **Threshold flavors.** That's why chips mix threshold flavors: low-threshold transistors only on the critical paths, high-threshold ones everywhere else to keep standby power down.

**Answer:** it leaks 17.8 times more.
:::
:::

::: check
given: T = 0.2 | 0.3 | 0.4; S = 65 | 80 | 100
answer: 1e-6*10^(-T/(S/1000))*1e12
unit: pA
tolerance: 0.5%

## A transistor's threshold, defined at 1 µA per µm, is {T} V and its swing {S} mV/decade. What does each micrometer of width leak at 0 V?

::: right
Right. $I_T \times 10^{-V_T/SS}$ = {answer} pA.
:::

::: misses
- [any] Not yet. Count the decades from threshold down to zero.
:::
:::

::: check
given: T = 77 | 300 | 400
answer: 8.617333e-5*T*ln(10)*1000
unit: mV
tolerance: 0.5%

## What's the smallest possible subthreshold swing at {T} K?

::: right
Right. $(kT/q)\ln 10$ = {answer} mV/decade.
:::

::: misses
- [8.617333e-5*T*1000] Multiply by ln 10 for a decade.
- [any] Not yet. The thermal limit.
:::
:::

::: check
given: t = 1.5 | 2 | 3; k = 9 | 22 | 25
answer: t*3.9/k
unit: nm
tolerance: 0.5%

## A gate dielectric is {t} nm thick with relative permittivity {k}. What's its equivalent oxide thickness?

::: right
Right. $t \times 3.9/\kappa$ = {answer} nm.
:::

::: misses
- [t*k/3.9] Higher κ gives a thinner equivalent oxide.
- [any] Not yet. Scale by the permittivities.
:::
:::

::: check
given: H = 40 | 50 | 60; W = 5 | 7; n = 1 | 2 | 3
answer: n*(2*H + W)
unit: nm
tolerance: 0.5%

## A FinFET has {n} fins, each {H} nm tall and {W} nm wide. What's its effective width?

::: right
Right. $n(2H_\text{fin} + W_\text{fin})$ = {answer} nm.
:::

::: misses
- [n*W] The gate wraps both sides and the top: the height counts twice.
- [any] Not yet. Add the gated sides of each fin.
:::
:::

::: check
kind: parts
given: S = 65 | 80 | 100; d = 50 | 100 | 150

## A transistor's subthreshold swing is {S} mV/decade, and its threshold is lowered by {d} mV.

::: part
answer: 10^(d/S)
tolerance: 0.5%

### By what factor does its leakage rise?

::: misses
- [any] $10^{\Delta V_T/S}$.
:::
:::

::: part
answer: S/(0.02585*ln(10)*1000)
tolerance: 0.5%

### How many times the 300 K limit of 59.5 mV/decade is its swing?

::: misses
- [any] S ÷ $(kT/q)\ln 10$.
:::
:::
:::

::: check
kind: parts
given: t = 5 | 7 | 10; x = 0.8 | 1; T = 77 | 300 | 373

## A fin of silicon {t} nm thick has {x} nm of oxide; the chip runs at {T} K.

::: part
answer: sqrt(11.7*t*x/(2*3.9))
unit: nm
tolerance: 0.5%

### What is its natural length?

::: misses
- [any] $\sqrt{\varepsilon_{Si}t_{Si}t_{ox}/(2\varepsilon_{ox})}$.
:::
:::

::: part
answer: 8.617e-5*T*ln(10)*1000
unit: mV
tolerance: 0.5%

### What is the subthreshold swing limit at {T} K?

::: misses
- [any] $(kT/q)\ln 10$.
:::
:::
:::

::: explain
## Why can't a conventional transistor switch more sharply than 60 mV per decade at room temperature?

::: model
Below threshold, a MOSFET conducts by letting electrons from the source climb over an energy barrier into the channel, and the number with enough thermal energy to get over falls off exponentially with the barrier height, by a factor of e for every kT of energy. The gate can at best lower the barrier by the full amount of its own voltage change, so a tenfold change in current needs the barrier to move by kT times ln 10, which is about 60 millielectronvolts at room temperature, and the gate voltage at least 60 millivolts. Wrapping the gate around the channel brings real devices close to this limit but not past it; only devices that don't rely on thermal emission, such as tunneling transistors, could.
:::
:::

::: practice

::: check
given: T = 0.1 | 0.5; S = 60 | 110
answer: 1e-6*10^(-T/(S/1000))*1e12
unit: pA
tolerance: 0.5%

## Leakage per µm: $V_T$ = {T} V, SS = {S} mV/dec?

::: misses
- [any] $I_T \times 10^{-V_T/SS}$.
:::
:::

::: check
given: t = 0.5 | 5; k = 7 | 40
answer: t*3.9/k
unit: nm
tolerance: 0.5%

## EOT of {t} nm at κ = {k}?

::: misses