---
title: "Modern transistors: high-κ gates, SOI, FinFETs and nanosheets"
heading: How the industry kept the gate in control of ever-shorter channels
eyebrow: S1 · Lesson 38 · Modern transistors
xp: 50
---

::: hook
By the mid-2000s the planar bulk MOSFET was out of room: its oxide leaked by tunneling, its doping fluctuated from transistor to transistor, and its gate couldn't hold short channels shut. Each fix was a materials or structural change. Hafnium oxide replaced silicon dioxide, metal replaced polysilicon, strained silicon sped up the carriers, and then the channel itself stood up on edge as a fin, wrapped by the gate on three sides. Today's transistors are stacks of horizontal nanosheets surrounded by gate on all four. This lesson works through the physics behind each step, so the jargon of a process roadmap reads as engineering.
:::

::: play
- DIBL against channel length for a 6 nm silicon body under 0.9 nm of equivalent oxide, with the gate on one side (thin-body SOI), two sides (double gate or FinFET) or all around (nanosheet or nanowire), on a log scale.
- More gates around the body shrink the natural length, so the drain's influence dies out faster and the same DIBL comes at a shorter channel.
- Thicken the body or the oxide and every curve shifts right: the gate's grip weakens.
:::
:::

```sim plot
view: graph
x: L = 5..60 nm
y: D = 1..1000 log
slider: tsi = 3..15 = 6 nm
slider: tox = 0.5..2 = 0.9 nm
plot: exp(-L/(2*sqrt(11.7*tsi*tox/3.9)))*1000 | samples: 400 | label: one gate (thin-body SOI), mV/V
plot: exp(-L/(2*sqrt(11.7*tsi*tox/(2*3.9))))*1000 | samples: 400 | color: ch2 | label: two gates (double gate, FinFET)
plot: exp(-L/(2*sqrt(11.7*tsi*tox/(4*3.9))))*1000 | samples: 400 | color: ch3 | label: gate all around (nanosheet)
marker: y = 50 | label: 50 mV/V
readout: natural length, one gate = sqrt(11.7*tsi*tox/3.9) nm
readout: natural length, all around = sqrt(11.7*tsi*tox/(4*3.9)) nm
```

::: predict
## Why did the industry move from planar transistors to FinFETs at around 22 nm?

- [ ] Fins conduct with higher mobility
- [ ] Fins are easier to manufacture
- [x] A gate wrapped around a thin fin controls the whole channel, shortening the natural length so short channels stay off
- [ ] Fins eliminate the need for a gate oxide

::: reveal
Electrostatic control. In a planar transistor the gate acts from one side and the channel's potential deep in the silicon is shared with the source and drain. A thin fin with gate on three sides has no deep silicon: every part of the channel is within a few nanometers of the gate. The natural length shrinks, so the same DIBL and swing come at a much shorter channel. As a bonus the fin can be undoped, removing random dopant variation, and its height adds drive current without adding footprint.
:::
:::

::: nameit
## High-κ dielectrics and metal gates

Direct tunneling through SiO₂ grows about tenfold for every 0.2 nm thinner, and below about 1.2 nm the gate leaks unacceptably. A material with higher permittivity gives the same capacitance in a thicker film:

$$\text{EOT} = t_{IL} + t_{HK}\frac{3.9}{\kappa_{HK}}$$

HfO₂-based films (κ ≈ 20 to 25) sit on a thin SiO₂ interfacial layer of about 0.5 nm, giving EOT under 1 nm with several nanometers of physical thickness. Polysilicon gates, whose depletion added 0.3 to 0.4 nm to the effective thickness and reacted with HfO₂, were replaced by metals chosen for their work functions: one near the conduction band for NMOS, one near the valence band for PMOS.

## Strain

Stretching silicon along the channel splits its conduction valleys and raises electron mobility; compressing it raises hole mobility. Silicon nitride liners and SiGe source-drain regions (whose larger lattice squeezes the channel) gave 30 to 80% more current with no change in size.

## Thin bodies and the natural length

With an undoped silicon body of thickness $t_{si}$ and n gates around it, the channel's potential settles over a natural length

$$\lambda \approx \sqrt{\frac{\varepsilon_s}{n\varepsilon_{ox}}t_{si}t_{ox}}$$

with n = 1 for thin-body SOI, 2 for a double gate or FinFET (the fin's top adds a little), and about 4 for a gate all around. The body thickness replaces the depletion depth, so thin bodies and more gates both help, and DIBL ≈ $e^{-L/2\lambda}$ as in lesson 37.

## Device structures

- **FD-SOI:** a 5 to 7 nm body on a thin buried oxide. The substrate under the oxide works as a back gate, so a bias there tunes the threshold, for speed or for low leakage.
- **FinFET:** fins about 5 to 8 nm wide and 40 to 50 nm tall. Each fin contributes about $2H_\text{fin} + W_\text{fin}$ of channel width, so width comes in whole fins.
- **Nanosheet (gate all around):** two to four horizontal sheets stacked and surrounded by gate. The sheets' width can vary continuously, unlike fins.
- **CFET** (in development): NMOS and PMOS stacked vertically.

## Variability

Small transistors differ from their neighbors. Random dopant counts, line-edge roughness and work-function grain differences give a threshold mismatch that follows **Pelgrom's law**,

$$\sigma_{\Delta V_T} = \frac{A_{VT}}{\sqrt{WL}}$$

with $A_{VT}$ about 1 to 2 mV·µm in modern processes. Undoped thin bodies cut the dopant part sharply. Analog designers make matched pairs large for this reason.
:::

::: example
## A gate stack has 0.5 nm of interfacial SiO₂ under 2 nm of HfO₂ (κ = 22). What's its EOT, and how much thinner would a plain SiO₂ gate of the same capacitance be?

::: solution
1. **EOT.**
   $$\begin{aligned} \text{EOT} &= 0.5 + 2 \times \frac{3.9}{22} \\ &= 0.85\ \text{nm} \end{aligned}$$
   against a physical thickness of 2.5 nm.
2. **Plain SiO₂ of the same capacitance.** It would be 0.85 nm thick, 1.65 nm thinner.
3. **Leakage.** By the rule of thumb (tenfold per 0.2 nm), that film would leak about $10^{8}$ times more than a 2.5 nm SiO₂ film.
4. **HfO₂'s own barrier.** HfO₂'s own tunneling barrier is lower than SiO₂'s, so the real gain is smaller, but still many orders of magnitude.

**Answer:** the EOT is 0.85 nm, so a plain SiO₂ gate of the same capacitance would be 1.65 nm thinner than the 2.5 nm stack.
:::
:::

::: example
## A 6 nm silicon body sits under 0.9 nm EOT. Compare the natural lengths and the DIBL at L = 16 nm for one gate, two gates and a gate all around.

::: solution
1. **Natural length with one gate.**
   $$\begin{aligned} \lambda &= \sqrt{\frac{11.7}{3.9} \times 6 \times 0.9}\ \text{nm} \\ &= 4.0\ \text{nm} \end{aligned}$$
2. **DIBL with one gate.**
   $$\begin{aligned} \text{DIBL} &= e^{-16/2\lambda} \\ &= 137\ \text{mV/V} \end{aligned}$$
3. **Two gates.** λ = 2.85 nm, and DIBL = 60 mV/V.
4. **Gate all around.** λ = 2.0 nm, and DIBL = 19 mV/V.
5. **Which is good enough.** Only the gate-all-around device is comfortably below 50 mV/V at this length, which is why the industry moved from fins to nanosheets as gate lengths approached 15 nm.

**Answer:** natural lengths of 4.0, 2.85 and 2.0 nm give DIBL of 137, 60 and 19 mV/V for one gate, two gates and a gate all around.
:::
:::

::: example
## Fins 50 nm tall and 7 nm thick sit on a 30 nm pitch. How much more width than a planar transistor does a FinFET fit in the same footprint?

::: solution
1. **Width per fin.** Each fin's gate wraps two sides and the top:
   $$2 \times 50 + 7 = 107\ \text{nm}$$
2. **Compare with planar.** That's 107 nm of width per 30 nm of pitch, 3.6 times the planar width.
3. **Taller fins.** Taller fins add drive current without using more area, at the cost of harder etching and more capacitance.

**Answer:** 3.6 times the planar width.
:::
:::

::: check
given: i = 0.3 | 0.6; t = 1.5 | 2.5 | 4; k = 16 | 25
answer: i + t*3.9/k
unit: nm
tolerance: 1%

## A gate stack has {i} nm of interfacial SiO₂ under {t} nm of a dielectric with κ = {k}. What's its EOT?

::: right
Right. $t_{IL} + t_{HK}\frac{3.9}{\kappa}$ = {answer} nm.
:::

::: misses
- [t*3.9/k] Add the interfacial layer: the two are in series.
- [any] Not yet. Convert the high-κ layer to its SiO₂ equivalent and add.
:::
:::

::: check
given: E = 0.7 | 0.9; i = 0.4 | 0.5; k = 18 | 25
answer: (E - i)*k/3.9
unit: nm
tolerance: 1%

## A target EOT of {E} nm must include {i} nm of interfacial SiO₂. How thick can the high-κ layer (κ = {k}) be?

::: right
Right. $(\text{EOT} - t_{IL})\frac{\kappa}{3.9}$ = {answer} nm.
:::

::: misses
- [E*k/3.9] Subtract the interfacial layer's share first.
- [any] Not yet. Solve the EOT formula for $t_{HK}$.
:::
:::

::: check
given: H = 40 | 50; W = 6 | 8; n = 1 | 2 | 4
answer: n*(2*H + W)
unit: nm
tolerance: 1%

## A FinFET has {n} fin(s), each {H} nm tall and {W} nm wide. What's its effective channel width?

::: right
Right. $n(2H_\text{fin} + W_\text{fin})$ = {answer} nm.
:::

::: misses
- [n*(H + W)] The gate covers both sides of each fin.
- [any] Not yet. Two sidewalls plus the top, per fin.
:::
:::

::: check
given: t = 5 | 10; o = 0.8 | 1.2; n = 2 | 3 | 4
answer: sqrt(11.7*t*o/(n*3.9))
unit: nm
tolerance: 1%

## A {t} nm body under {o} nm EOT has {n} gate(s) around it. What's its natural length?

::: right
Right. $\sqrt{\frac{\varepsilon_s}{n\varepsilon_{ox}}t_{si}t_{ox}}$ = {answer} nm.
:::

::: misses
- [sqrt(11.7*t*o/3.9)] Divide by the number of gates.
- [any] Not yet. Use the natural-length formula.
:::
:::

::: check
given: A = 1 | 2.5; W = 0.05 | 0.2 | 1; L = 0.02 | 0.1
answer: A/sqrt(W*L)
unit: mV
tolerance: 1%

## A process has $A_{VT}$ = {A} mV·µm. What threshold mismatch (one standard deviation) does a pair of transistors {W} µm × {L} µm have?

::: right
Right. $\frac{A_{VT}}{\sqrt{WL}}$ = {answer} mV.
:::

::: misses
- [A/(W*L)] Mismatch falls with the square root of the area.
- [any] Not yet. Use Pelgrom's law.
:::
:::

::: check
given: u = 250 | 400; s = 30 | 60; L = 20 | 100
answer: (1 + s/100)*(1 + 0.5*u/(2e7*L*1e-7))/(1 + 0.5*u*(1 + s/100)/(2e7*L*1e-7))
tolerance: 1%

## Strain raises the mobility of a transistor (L = {L} nm, μ = {u} cm²/(V·s), $v_{sat} = 10^7$ cm/s) by {s}%. At an overdrive of 0.5 V, by what factor does its saturation current rise?

::: right
Right. With $I \propto \frac{\mu}{1 + V_{ov}\mu/2v_{sat}L}$, the current rises by {answer}: less than the mobility, because velocity saturation caps part of the gain.
:::

::: misses
- [1 + s/100] That's the long-channel answer; velocity saturation cuts the benefit.
- [any] Not yet. Use the velocity-saturation model of lesson 37 with both mobilities.
:::
:::

::: check
given: d = 0.3 | 0.4 | 0.6
answer: 10^(d/0.2)
tolerance: 2%

## Gate tunneling through SiO₂ grows about tenfold for every 0.2 nm thinner. By what factor does it grow if the oxide thins by {d} nm?

::: right
Right. $10^{\Delta t/0.2\text{ nm}}$ = {answer}.
:::

::: misses
- [10*d/0.2] Each 0.2 nm multiplies by ten: exponential, not linear.
- [any] Not yet. Count the 0.2 nm steps.
:::
:::

::: check
kind: parts
given: h = 30 | 50 | 70; t = 5 | 7; p = 25 | 30 | 45

## Fins {h} nm tall and {t} nm thick sit on a {p} nm pitch.

::: part
answer: 2*h + t
unit: nm
tolerance: 0.5%

### What effective width does each fin give?

::: misses
- [h + t] The gate wraps both sides and the top.
- [any] $2h + t$.
:::
:::

::: part
answer: (2*h + t)/p
tolerance: 0.5%

### How many times the planar width fits in the same footprint?

::: misses
- [any] Width ÷ pitch.
:::
:::
:::

::: check
kind: derivation
vars: a = 1e-8..2e-7, b = 1e-8..1e-6, k = 10..30

## A gate stack has a SiO₂ interlayer of thickness a under a high-κ layer of thickness b with permittivity κ = k.

::: step
answer: a + b*3.9/k

### What is its EOT?
:::

::: step
answer: 3.45e-13/(a + b*3.9/k)

### What capacitance per cm² does it give?
:::

::: right
Right. The interlayer counts in full, so it sets a floor on EOT however good the high-κ layer is.
:::
:::

::: explain
## Why does wrapping the gate around more sides of a thin channel let the transistor's channel be shorter?

::: model
A short channel fails when the source and drain fields reach the middle of the channel and lower the barrier there, competing with the gate. How far those fields reach is set by the natural length: the distance over which the gate can pull the channel's potential back to its own value. That length depends on how much silicon lies between the gate and the farthest part of the channel, and how strongly the gate is coupled through its oxide. A gate on one side of a thick body leaves silicon far from the gate where the drain's field dominates. A thin body with gates on two, three or four sides has no such region, so the natural length shrinks and the drain's influence dies out within a few nanometers.
:::
:::

::: practice

::: check
given: i = 0.35 | 0.55; t = 1.8 | 3; k = 20 | 23
answer: i + t*3.9/k
unit: nm
tolerance: 1%

## EOT: {i} nm SiO₂ + {t} nm at κ = {k}?

::: misses
- [any] $t_{IL} + t_{HK}(3.9/\kappa)$.
:::
:::

::: check
given: t = 4 | 7; o = 0.9 | 1.1; n = 2 | 4
answer: sqrt(11.7*t*o/(n*3.9))
unit: nm
tolerance: 1%

## Natural length: {t} nm body, {o} nm EOT, {n} gates?

::: misses
- [any] $\sqrt{3t_{si}t_{ox}/n}$.
:::
:::

::: check
given: A = 1.2 | 3; W = 0.1 | 0.5; L = 0.05 | 0.2
answer: A/sqrt(W*L)
unit: mV
tolerance: 1%

## Pelgrom mismatch: $A_{VT}$ = {A} mV·µm, {W} × {L} µm?

::: misses
- [any] $A_{VT}/\sqrt{WL}$.
:::
:::
:::
