S1 · Lesson 33 · MOS C–V curves and oxide charges
Reading a capacitor's curve for oxide thickness, doping and trapped charge
Sweep the gate voltage of a MOS capacitor and measure its small-signal capacitance, and you get a curve that fabs measure on test structures from almost every wafer. Its top gives the oxide thickness, its bottom the substrate doping, and its position along the voltage axis the charge trapped in the oxide. A stretched-out step means the interface has defects; a curve that moves after heating under bias means mobile sodium got in. The capacitor is the cheapest, most sensitive probe of a gate stack there is.
- Capacitance (÷ ) against gate voltage for an n⁺ poly gate on p-type silicon, in the depletion approximation: high frequency (solid), low frequency (dashed) and a fast sweep that drives the surface into deep depletion.
- In accumulation the capacitance is . In depletion the depletion layer adds a second capacitor in series and C falls. Past threshold, the low-frequency curve climbs back to as the inversion layer follows the signal; the high-frequency curve stays at its minimum.
- Add positive fixed charge to the oxide: the whole curve shifts left without changing shape. Thin the oxide and the dip becomes shallower.
Predict
Positive charge is trapped in a MOS capacitor's oxide, near the silicon. Which way does its C–V curve move?
Toward negative voltages. Positive charge near the interface already pulls electrons toward the surface and repels holes, doing part of the gate's job. The gate needs that much less positive voltage (or more negative voltage) to reach each point of the curve, so the whole curve shifts by . A positive shift means negative trapped charge, which is what hot electrons injected into the oxide produce as a transistor wears out.
Name it
The curve, region by region
- Accumulation: holes at the surface respond instantly, so .
- Flat band: the surface charge responds over a Debye length, .
- Depletion: the depletion layer is a second capacitor in series, , which in the depletion approximation is .
- Inversion, low frequency: electrons are generated fast enough to follow the signal (below about 10 Hz), and the capacitance returns to .
- Inversion, high frequency: they can't, so only the depletion edge moves and , with .
- Deep depletion: a sweep faster than generation can supply electrons lets the depletion region keep widening past .
So gives , and gives and from it .
Charges in and near the oxide
- Fixed charge , positive, in the first nanometer of oxide: . About to q/cm² in good thermal oxide.
- Mobile ions (Na⁺, K⁺) drift through the oxide when heated under bias, so the curve moves after bias-temperature stress. A charge sheet at distance x from the gate shifts flat band by : none when it's at the gate, the full amount at the silicon.
- Oxide trapped charge from radiation or hot-carrier injection.
- Interface traps (per cm² per eV) charge and discharge as the surface potential sweeps through them, so each step of takes extra gate voltage : the curve stretches out. Good Si/SiO₂ has near cm⁻²eV⁻¹ after a hydrogen anneal.
Flat band and the work function
An n⁺ gate and a p⁺ gate differ in by about the band gap, 1.1 V, which is why CMOS long used n⁺ poly for NMOS and p⁺ poly for PMOS, and why metal gates are chosen by work function.
Worked example
A capacitor of area cm² measures 172.7 pF in accumulation and 28.5 pF at its high-frequency minimum. Its flat band sits at −1.13 V with an n⁺ poly gate. Find , and the fixed charge.
Show the solution
- Oxide thickness. = 1.727 × 10⁻⁷ F/cm², so
- Depletion width from the minimum. With both capacitances per area,
- Doping. Since depends on through too, iterate It settles at cm⁻³.
- Work-function difference.
- Fixed charge. The extra −0.213 V means or 2.3 × 10¹¹ charges per cm².
Answer = 20 nm and cm⁻³, and the fixed charge is C/cm², or charges per cm².
Worked example
A bias-temperature test drives Na⁺ ions per cm² from the gate side of a 20 nm oxide to the silicon side. How far does flat band move?
Show the solution
- At the gate. At the gate side the ions had no effect.
- At the silicon. There they shift flat band by
- Oxide thickness. A thinner oxide would hide the same contamination better (larger ), which is one reason mobile-ion tests use thick test oxides.
Answer flat band moves by −0.093 V.
Worked example
A 20 nm oxide carries cm⁻² of fixed positive charge at the interface. How far does it shift the flat-band voltage?
Show the solution
- Oxide capacitance.
- Flat-band shift.
- Thinner oxides. Thinner oxides shrink the shift in proportion, which is part of why thin gates tolerate imperfect interfaces.
Answer −46 mV.
Check
An oxide 2 nm thick holds 1 × 10¹¹ fixed positive charges per cm² at the silicon interface. How much do they shift flat band?
Write units the way you normally would: 1.5 V, 1500 mV and 0.0015 kV are the same answer.
Check
A MOS capacitor of area 0.0001 cm² measures 200 pF in accumulation. How thick is its oxide?
Write units the way you normally would: 1.5 nm, 1500 pm and 0.0015 µm are the same answer.
Check
What's the high-frequency for 5 nm of oxide on p-type silicon doped 1 × 10¹⁵ cm⁻³?
Check
A sheet of 5 × 10¹⁰ positive charges per cm² sits at 0.5 of the way from gate to silicon in a 30 nm oxide. How much does it shift flat band?
Write units the way you normally would: 1.5 V, 1500 mV and 0.0015 kV are the same answer.
Check
An interface with = 1 × 10¹¹ cm⁻²eV⁻¹ sits under 2 nm of oxide. How much extra gate voltage does it take to sweep the surface potential 0.5 V?
Write units the way you normally would: 1.5 mV, 1500 µV and 0.0015 V are the same answer.
Check
A capacitor with 5 nm of oxide on p-type silicon ( = 1 × 10¹⁷) is 0.5 V above flat band, still below threshold. What's C/?
Check
What's the flat-band capacitance, as a fraction of , for 10 nm of oxide on silicon doped 1 × 10¹⁵ cm⁻³?
Check
An oxide 10 nm thick carries cm⁻² of fixed positive charge at its interface, Q = 1.
(a)
What is ?
Write units the way you normally would: 1.5 nF/cm², 1500 pF/cm² and 0.0015 µF/cm² are the same answer.
(b)
How far does flat band shift?
Check
A MOS capacitor of area A (cm²) measures Ca pF in accumulation and Cm pF at its high-frequency minimum.
Step 1
What is the oxide thickness, in cm?
Type it the way you would write it, like 3sin(2πft) or 3*sin(2*pi*f*t). Angles can be in radians or carry a degree sign, like 45°.
Step 2
What is the depletion capacitance at the minimum, in farads?
Step 3
What is the maximum depletion width, in cm?
Explain why
Why does a MOS capacitor's capacitance return to in inversion at low frequency but not at high frequency?
In inversion, a small change in gate voltage can be answered either by electrons joining or leaving the inversion layer right at the surface, or by the depletion edge moving deep in the silicon. Electrons right at the surface make the capacitor look like the oxide alone, . But the inversion electrons have to come from somewhere: in a capacitor there's no source, so they must be generated thermally, which takes time. At low frequency there's enough time and the inversion layer follows the signal. At high frequency it can't, so the depletion edge moves instead, and the capacitance stays at the series combination of the oxide and the maximum depletion layer. In a MOSFET the source supplies electrons instantly, so its gate shows the low-frequency curve at any normal frequency.
Practice
Keep practicing
11 kinds of problem on this topic, dealt one at a time with new numbers every time, for as long as you like.